如何保證壓制的C型鋼不厚均勻?

來源:http://www.ebassfish.com/ 日期:2021-04-22 發布人:jiangucaigang
不同用戶,對于C型鋼壁的厚度要求也是不同的,有的會比較后,有些卻是非常的薄。如果要同時滿足這些要求的話,所選用的C型鋼生產工藝和設備非常關鍵。據小編所知,一般了冷軋方式是難以生產出高品質的C型鋼,因此得用C型鋼機來完成。
Different users have different requirements for the thickness of C-section steel wall. Some will be compared, but some are very thin. If we want to meet these requirements at the same time, the selected C-beam production process and equipment is very critical. As far as Xiaobian knows, it is difficult to produce high quality C-beam by cold rolling, so it has to be finished by C-beam machine.
材料從C型鋼機的尾部進入之后,經過各種壓輥的壓制,從頭部輸出成型后的C型鋼。這不僅使得必要的生產加工工藝得到了極大的優化,同時提高了生產下來,還能保證C型鋼產品具有均勻的壁厚和復雜的界面形狀。
After the material enters from the tail of the C-beam machine, it is pressed by various rollers, and the shaped C-beam is output from the head. This not only makes the necessary production process has been greatly optimized, but also improves the production efficiency, and ensures that C-beam products have uniform wall thickness and complex interface shape.
為了達到精確的壁厚,C型鋼機在壓制C型鋼的時候,使用的模具是由一個精準的上模和一些大小規格尺寸相同的下模構成的。在加工之前將它們安裝到位,不僅要保證上模與下模能夠順利的,還得確保四周邊間隙均勻,這樣壓制的C型鋼才能壁厚均勻。
In order to achieve accurate wall thickness, the mold used by C-beam machine in pressing C-beam is composed of an accurate upper mold and some lower molds with the same size. Before processing, they should be installed in place, not only to ensure the smooth operation of the upper and lower dies, but also to ensure the uniform clearance around the four edges, so that the pressed C-beam can have uniform wall thickness.
此文關鍵詞: 濟南C型鋼廠  

推薦閱讀/ Recommended reading

相信大家對彩鋼復合板都不會陌生,畢竟在生活中是比較常見的。雖然濟南彩鋼復合板引進不到20年時間,但由于其具有承力、保溫隔熱、裝飾、防

防火彩鋼板表面為什么出現壓斑? 2022-02-26
有哪些原因會導致C型鋼出現變形的現象? 2022-02-22
彩鋼瓦具有哪些優勢? 2022-02-17
復合板質量控制的措施及建議 2022-02-14
欧美激情视频-人妻av综合天堂一区-色天使色妺妺网站-无码a片